JPH0535203B2 - - Google Patents
Info
- Publication number
- JPH0535203B2 JPH0535203B2 JP16338385A JP16338385A JPH0535203B2 JP H0535203 B2 JPH0535203 B2 JP H0535203B2 JP 16338385 A JP16338385 A JP 16338385A JP 16338385 A JP16338385 A JP 16338385A JP H0535203 B2 JPH0535203 B2 JP H0535203B2
- Authority
- JP
- Japan
- Prior art keywords
- forging
- gear
- spur gear
- strength
- warm
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Preventing Corrosion Or Incrustation Of Metals (AREA)
- Forging (AREA)
- Solid-Phase Diffusion Into Metallic Material Surfaces (AREA)
- Heat Treatment Of Steel (AREA)
- Heat Treatment Of Articles (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16338385A JPS6223930A (ja) | 1985-07-23 | 1985-07-23 | 高強度平歯車の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16338385A JPS6223930A (ja) | 1985-07-23 | 1985-07-23 | 高強度平歯車の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6223930A JPS6223930A (ja) | 1987-01-31 |
JPH0535203B2 true JPH0535203B2 (en]) | 1993-05-26 |
Family
ID=15772841
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP16338385A Granted JPS6223930A (ja) | 1985-07-23 | 1985-07-23 | 高強度平歯車の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6223930A (en]) |
Families Citing this family (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6418545A (en) * | 1987-07-14 | 1989-01-23 | Honda Motor Co Ltd | Method for forging gear |
JP2709596B2 (ja) * | 1988-02-05 | 1998-02-04 | 株式会社豊田中央研究所 | 肌焼鋼強靭部品の製造方法 |
JP5200634B2 (ja) | 2007-04-11 | 2013-06-05 | 新日鐵住金株式会社 | 鍛造及び浸炭用熱間圧延棒鋼 |
CN104668433A (zh) * | 2015-02-03 | 2015-06-03 | 江苏金源锻造股份有限公司 | 一种大齿轮的锻造工艺 |
CN104972037A (zh) * | 2015-06-24 | 2015-10-14 | 陈文建 | 一种改善锻件表面质量的锻造工艺 |
CN104972036A (zh) * | 2015-06-24 | 2015-10-14 | 陈文建 | 一种工件锻造工艺 |
CN107470528B (zh) * | 2017-08-04 | 2019-02-01 | 钢铁研究总院 | 一种核电用SA508Gr.4N钢大锻件中心部位细化的锻造方法 |
CN107699671B (zh) * | 2017-08-05 | 2019-01-04 | 福州思琪科技有限公司 | 一种雪橇合金滑板用型钢 |
-
1985
- 1985-07-23 JP JP16338385A patent/JPS6223930A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6223930A (ja) | 1987-01-31 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP5729213B2 (ja) | 熱間プレス部材の製造方法 | |
JPS6043431B2 (ja) | 軽荷重用窒化機械部品の製造法 | |
JPH0953149A (ja) | 高強度高靭性肌焼き用鋼 | |
JPH0325253B2 (en]) | ||
JPH0535203B2 (en]) | ||
JP4266341B2 (ja) | 冷間鍛造性及び肌焼処理時の耐粗粒化特性に優れた球状化焼鈍省略肌焼用鋼及びその製造方法 | |
JPS589813B2 (ja) | 非調質鍛鋼品の製造方法 | |
JP2000063935A (ja) | 窒化部品の製造方法 | |
JPS5967365A (ja) | 機械部品の製造方法 | |
JP3550886B2 (ja) | 被削性および疲労強度に優れた高周波焼入用の歯車用鋼材の製造方法 | |
JP2549039B2 (ja) | 歪の小さい高強度歯車の浸炭窒化熱処理方法 | |
JPH10226817A (ja) | 軟窒化用鋼材の製造方法及びその鋼材を用いた軟窒化部品 | |
JP3623313B2 (ja) | 浸炭歯車部品 | |
JP2549038B2 (ja) | 歪の小さい高強度歯車の浸炭熱処理方法およびその歯車 | |
JPS6144159A (ja) | 浸炭窒化性にすぐれた冷間鍛造用鋼 | |
JP6583484B2 (ja) | 窒化用鋼 | |
JPH09279296A (ja) | 冷間鍛造性に優れた軟窒化用鋼 | |
JP3109146B2 (ja) | 低歪高強度部材の製造方法 | |
JPH0754041A (ja) | 冷間鍛造用鋼の製造方法 | |
JP3264790B2 (ja) | 異形断面を有する引抜き部品とその製造方法 | |
JPH0227408B2 (en]) | ||
JP7310723B2 (ja) | 鋼部品およびその製造方法 | |
JPS60262941A (ja) | 温間鍛造用鋼 | |
JPH08291371A (ja) | 表面に高強度層を有する鍛造部品及びその製造方法 | |
KR100501680B1 (ko) | 기어용 보론 합금강의 열처리 방법 |